Simple routes from natural graphite to graphite foams: Preparation, structure and properties 期刊论文
CARBON, 2020, 卷号: 159, 页码: 527-541
Authors:  Duan, Shengzhi;  Wu, Xiaowen;  Zeng, Keqing;  Tao, Tianyi;  Huang, Zhaohui;  Fang, Minghao;  Liu, Yangai;  Min, Xin
Favorite  |  View/Download:11/0  |  Submit date:2020/05/21
Graphite foams  Natural flake graphite  Thermal diffusivity  Sucrose  NaCl template  
Electrolytic preparation and characterization of VCr alloys in molten salt from vanadium slag 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 卷号: 803, 页码: 875-881
Authors:  Liu, Shiyuan;  Wang, Lijun;  Chou, Kuo-chih;  Kumar, Ramachandran Vasant
Favorite  |  View/Download:37/0  |  Submit date:2019/10/18
VCr alloy  Electrodeposition  NaCl-KCl-VCl3-CrCl3 molten salt  
Direct electrolytic preparation of chromium metal in CaCl2-NaCl eutectic salt 期刊论文
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2018, 卷号: 28, 期号: 2, 页码: 376-384
Authors:  Liu, Zheng-wei;  Zhang, Hong-ling;  Pei, Li-li;  Shi, Yi-lang;  Cai, Zai-hua;  Xu, Hong-bin;  Zhang, Yi
Favorite  |  View/Download:99/0  |  Submit date:2018/06/11
Electrolysis  Chromium  Chromium Oxide  Cacl2-nacl Molten Salt  
Hot corrosion of Ni, Cr, and 80Ni20Cr in the presence of NaCl and water vapor at 750 degrees C 期刊论文
MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2017, 卷号: 68, 期号: 11, 页码: 1172-1179
Authors:  Chen, L. Y.;  Lan, H.;  Huang, C. B.;  Yang, B.;  Du, L. Z.;  Zhang, W. G.
Adobe PDF(1737Kb)  |  Favorite  |  View/Download:63/0  |  Submit date:2017/12/20
Hot Corrosion  Nacl  Synergistic Effect  Water Vapor  
Electrochemical Preparation of V2O3 from NaVO3 and Its Reduction Mechanism 期刊论文
JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2017, 卷号: 32, 期号: 5, 页码: 1019-1024
Authors:  Weng Wei;  Wang Mingyong;  Gong Xuzhong;  Wang Zhi;  Wang Dong;  Guo Zhancheng
Adobe PDF(1405Kb)  |  Favorite  |  View/Download:117/0  |  Submit date:2017/11/27
Molten Salt Electrolysis  V2o3  Navo3  Molten Nacl  
Hot corrosion behavior of porous nickel-based alloys containing molybdenum in the presence of NaCl at 750 degrees C 期刊论文
ENGINEERING FAILURE ANALYSIS, 2017, 卷号: 79, 期号: SEP, 页码: 245-252
Authors:  Chen, Lingyun;  Lan, Hao;  Huang, Chuanbing;  Yang, Bin;  Du, Lingzhong;  Zhang, Weigang
Adobe PDF(1516Kb)  |  Favorite  |  View/Download:97/0  |  Submit date:2017/09/06
Nicrmo  Hot Corrosion  Oxidation  Nacl  
多孔NiCr在750℃ NaCl沉积盐中的热腐蚀机理研究 期刊论文
航空制造技术, 2017, 期号: 08, 页码: 32-36
Authors:  陈凌云;  兰昊;  黄传兵;  杨滨;  房师阁;  张伟刚
Adobe PDF(3160Kb)  |  Favorite  |  View/Download:179/0  |  Submit date:2018/09/05
Nacl  热腐蚀  涂层  多孔nicr  
AlCl_3-NaCl复盐为铝源电解共沉积制备镁铝合金 期刊论文
过程工程学报, 2017, 卷号: 17, 期号: 05, 页码: 1072-1077
Authors:  刘洋;  卢旭晨;  张志敏;  陈世伟
Adobe PDF(1090Kb)  |  Favorite  |  View/Download:68/0  |  Submit date:2018/09/05
Alcl3-nacl复盐  电解共沉积  Mgcl2·6h2o  镁铝合金  
Determination and Modeling of Solubility for CaSO4 center dot 2H(2)O-NH4+-Cl--SO42--NO3--H2O System 期刊论文
JOURNAL OF CHEMICAL AND ENGINEERING DATA, 2012, 卷号: 57, 期号: 12, 页码: 3664-3671
Authors:  Tian, Ping;  Ning, Pengge;  Cao, Hongbin;  Li, Zhibao;  Cao, HB
Adobe PDF(661Kb)  |  Favorite  |  View/Download:248/9  |  Submit date:2013/10/08
Calcium-sulfate Solubility  Waste-water Streams  hcl+cacl2 Solutions  Ammonium-sulfate  Caso4 Phases  Degrees-c  353 k  Removal  Gypsum  Nacl  
Corrosion of several typical alloys in concentrated sodium alumiate solution with chloride Na_2O-Al_2O_3-NaCl-H_2O system at 180-240℃ 会议论文
第二届中国科学院博士后学术年会暨高新技术前沿与发展学术会议程序册, 中国海南三亚, 2010-03-25
Authors:  Ju SH(巨少华)
Adobe PDF(72Kb)  |  Favorite  |  View/Download:155/0  |  Submit date:2013/09/29
Chloride:9059  Typical:4131  Solution:487  Concentrated:449  Sodium:360  Alloys:354  Several:341  System:209  Nacl:61